Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2731
We recently had some boards returned that have me stumped. W... - Aug 18, 2005 by
Sounds to me like you have one of two problems. First would ... - Aug 24, 2005 by Avalancher
Sounds like a part problem with me too. I would suspect that... - Aug 24, 2005 by
Hi MM, Off the cuff, is it possible that the QFP leads w... - Aug 25, 2005 by
Agree with Dan - we have had non-plated IC's that are a bit ... - Aug 25, 2005 by
Could it be cold solder? Are there parts nearby that might ... - Aug 25, 2005 by Stephen
I would attack the simplest possibility first. Make SURE you... - Aug 25, 2005 by Steve Thomas
Hi, Wanna to know if you have extra boad (Solder Sample) ... - Aug 29, 2005 by
what is the plating on the component ? Lead free ? ... - Aug 29, 2005 by
All of your response were similar to our investigation. Past... - Aug 30, 2005 by
The parts could still be the problem regardless if they came... - Sep 01, 2005 by adlsmt
MM