Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2878
Hello, I have a question on white residues formation at w... - Aug 16, 2005 by
Hi, Are they no clean fluxes? Regards, Grant ... - Aug 16, 2005 by Grant
Peter: Questions are: * From your pictures, the white resid... - Aug 16, 2005 by davef
It appears that the flux was burnt over the wave process. I... - Aug 16, 2005 by RDR
Hi Peter, I posted these links to Technet as well, but figu... - Aug 16, 2005 by sarag
Dave, Answers to your questions: * From your picture... - Aug 17, 2005 by Peter
What is the surface finish of the board ? Some flux are know... - Aug 17, 2005 by
As others said, it appears that this mask and than flux are ... - Aug 17, 2005 by davef