Lead Free parts in Lead solder

wbfranklin

#33227

Lead Free parts in Lead solder | 16 March, 2005

Hello all,

I've heard mixed reviews on this subject. Can anyone point out some data on the integrity of lead free parts that are soldered with lead solder. I think that we're probably ALL running into this during this Pb-free transition period.

There's lots of data out there on complete Pb-free v.s. SnPB, but I've found that people aren't too forthcoming with their knowledge on this "mixed technology" subject...

Thanks in advance!

Will

This message was posted via the Electronics Forum @

reply »

pr

#33229

Lead Free parts in Lead solder | 16 March, 2005

I think this has been discussed on a couple of recent threads. Check recent archives.

good luck, pr

reply »

leon

#33230

Lead Free parts in Lead solder | 16 March, 2005

hi,

what we have learnt is lead free parts are ok to use with lead solder except BGA where you have to be carefull at reflow.

reply »


RDR

#33233

Lead Free parts in Lead solder | 16 March, 2005

This condition has been discussed on numerous occasions in this forum. Please do a search in the archives. Anyway, the manufacturing industry has been using lead free parts for at least ten years with lead paste. It is the other way around that is not so good.

reply »

chon

#33415

Lead Free parts in Lead solder | 28 March, 2005

How can I look into "archives" regarding to lead free threads?

reply »


RDR

#33416

Lead Free parts in Lead solder | 28 March, 2005

Type in "lead free" and search in forum in the search box at the top of this screen.

reply »

chon

#33434

Lead Free parts in Lead solder | 29 March, 2005

Thanks I'am kinda new user in this forum

reply »