Hi All,

could anyone advise me what we need to pay attention to if we will be usingthe Sn Pin plating as lead free requirement in SMT reflow process, is it a need to increase the Temp Profile by 10~15 Degree c as Sn with Melting ppoint 232C,

Please share your experience with us!

reply »

#32193

QFP with Sn Pin Plating | 21 January, 2005

Your first point of focus should be the thermal recipe recommendations of your paste supplier.

reply »

WDLau

#32217

QFP with Sn Pin Plating | 24 January, 2005

we are using SAC305 solder paste