Conformal coating application

JDumont

#30715

Conformal coating application | 27 September, 2004

Morning all, Can anyone recommend a simple low cost method to spray apply conformal coating to our PCB's. Looking for something simple, semi-automatic, and repeatable for operators to use without problems. This is a very low volume application, approx one 40 board batch per month. Thanks in advance... JD

reply »

HOSS

#30726

Conformal coating application | 27 September, 2004

JD,

Have you considered manual dipping? For that low of a volume, the purchase cost and maintenance wouldn't seem economical but I'm not in your shoes.

With hand dipping, you don't have the thickness control you may need but it can be done. If your application doesn't get too tight with thickness tolerances, you might give the manual method a look. Just make sure you have good ventilation and understand your local environmental requirements.

reply »

#30730

Conformal coating application | 27 September, 2004

We agree with Hoss. Dipping is far more controllable and less expensive than spraying for the casual user. An alternative to consider contracting your coating requirements. Amoung the service providers are: * http://www.newenglandcoating.net

* http://www.advancedcoating.com

Your coating materials supplier can give you a fairly straight skinny on the costs and facilities requirements for varous alternatives.

reply »

#30731

Conformal coating application | 27 September, 2004

Hi,

You may look into PVA 650 which cost around US$40K for a unit. Let me know which company you are or which location will you be and I shall get my team to visit you and let you know more about this sysytem.

Regards Danny Hui

reply »

#30732

Conformal coating application | 27 September, 2004

Danny: Beyond the US$40k that you mention for the machine, how much money should be budgeted for: * Facilities cost for spray room contruction, venting / filtration, fire proofing, etc? * Operating costs, such as training, maintenance, operation, etc? * Other costs, not mentioned

reply »

#30749

Conformal coating application | 28 September, 2004

Hey guys, I would be looking for something along the lines of the PVA 250 model, VERY basic....

reply »

blnorman

#30794

Conformal coating application | 30 September, 2004

I'll third the motion for hand dipping the boards. One other idea is to get coating in a can. Many companies will supply coatings in aerosol cans for touch up and small usage.

reply »

#30936

Conformal coating application | 12 October, 2004

Ok, so as it turns out our vendor may be buying us the dispensing system to you on their product. Any suggestions now for a system in the 25K range....things are looking up!

reply »

#30954

Conformal coating application | 13 October, 2004

Good morning. We have a used Nordson Coater, Batch type (not pass thru), w/o cure oven,that you can purchase for $9,950.00. Unit has been cleaned and lines purged. It was running when decommissioned, and is still in nice shape. Thanks, Nick Haviland. Electronic Assembly Machinery Exchange. email me at ----eamexco@sbcglobal.net for picts.

reply »

#30955

Conformal coating application | 13 October, 2004

Consider: * Equipment||Coating dip tank||Glenpro (2143 dip tank)||39 McBride Ave., Paterson, NJ 07501-1715 * Equipment||Coating dip tank||CCRCo||1954 Placentia Ave. Suite 107 Costa Mesa, CA 92627||800-443-2726 949-574-1360 Fax 1368 info@CCRCo.com http://www.ccrco.com

* Equipment||Coating dip tank||Inseto (UK) Limited; Unit 25, Focus 303, Focus Way, Andover, Hants SP10, 5NW, UK||+44(0) 1264 334505, Fax: +44(0) 1264 334449 http://www.inseto.co.uk enquiries@inseto.co.uk

reply »