I am looking for some tips of the trade with solder charges.... - Aug 07, 2023 by QA123
To resolve this issue, we use stencils with a step in the l... - Aug 08, 2023 by dima
Did you struggle with bridging? ... - Aug 08, 2023 by QA123
What thickness did you go to and what aperture size did you ... - Aug 08, 2023 by QA123
We use 7mil step 35mil diameter. Never got a bridges problem... - Aug 09, 2023 by dima
thanks we will give it a try ... - Aug 09, 2023 by QA123
For which connectors? We are using a Andon BGA connector and... - Aug 10, 2023 by leeg
We are using a SAMTEC BGA connector. ... - Aug 10, 2023 by dima