I'm looking at some Pillarhouse and Juki machines used. Does... - Jan 23, 2023 by Poly
Try to stay away from this process in general. I have worked... - Jan 23, 2023 by Evtimov
Have you looked at simple solder fountains? If it is just si... - Jan 23, 2023 by Stephen
There is alot to talk about. I have used a couple different ... - Jan 23, 2023 by bobpan
Emtimov, what are you using instead? Hand soldering? Is the ... - Jan 24, 2023 by Poly
"Try to stay away from this process in general. I have ... - Jan 24, 2023 by dontfeedphils
I have been involved with our Selective Soldering process fo... - Jan 24, 2023 by ProcEng1
What about nitrogen purity? Erza won't say anything other th... - Jan 24, 2023 by Stephen
I'm mostly thinking of a Juki or a Pillarhouse, is the Juki ... - Jan 25, 2023 by Poly
We have only had our Juki about 6 months, but it seems to be... - Jan 25, 2023 by ProcEng1
I'm now looking at Juki / Inertec and Ebso. I can get a used... - Jan 27, 2023 by Poly