Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2383
Smt juki 2060 is constantly throwing Tombstone error message... - Jan 09, 2023 by CrystalW
Check your 500 nozzles under a microscope very closely for t... - Jan 10, 2023 by Sr. Tech
Okay that makes sense actually. I was under that impression ... - Jan 10, 2023 by CrystalW
Also small quantities of solder paste can work its way into ... - Jan 11, 2023 by sarason
We have issues with different Juki machines needing differen... - Jan 12, 2023 by leeg
Interesting. Thank uou ... - Jan 12, 2023 by CrystalW
There are a couple of things you can try that seemed to help... - Jan 13, 2023 by Servin