I have modules that come with a 4 x 2 pin header. The proble... - Sep 23, 2020 by SMTA-64387098 SMTA
Try to pre-tin the part. This should give you a lot of answe... - Sep 23, 2020 by Evtimov
In my opinion, it is not possible to eliminate the oxidation... - Sep 24, 2020 by Djo
If whatever is preventing the leads on your component from w... - Sep 24, 2020 by davef