I'm having a problem getting sufficient solder reflow on a S... - Aug 13, 2020 by IronSMT
Is that no solder on the left hand pins in the picture? If ... - Aug 13, 2020 by robgd3
Thanks for the feedback Rob, Yes that is a no solder. Ther... - Aug 13, 2020 by IronSMT
Are you getting the same solder issues on all of the compone... - Aug 13, 2020 by robgd3
We understand you can't change the board design, but can you... - Aug 14, 2020 by Evtimov