we have a problem : The connector is falling down in the sec... - Feb 11, 2020 by Djo
If all else fails, you can always chipbond the part. Would ... - Feb 11, 2020 by dontfeedphils
To predict whether or not a first pass part is going to come... - Feb 11, 2020 by Steve Thomas
Hi there , I agree with phil .. but we cannot change the ar... - Feb 12, 2020 by Djo
If you have control of the solder alloy you're able to use o... - Feb 12, 2020 by dontfeedphils
We can't do that because we are using dual ligne reflow oven... - Feb 12, 2020 by Djo
Would you consider a light reflow pallet on second side hold... - Feb 12, 2020 by Evtimov
Would you consider a light reflow pallet on second side hold... - Feb 12, 2020 by Evtimov
we have already taken this idea into consideration but as a ... - Feb 12, 2020 by Djo
No to redesign, no to glue dispensing and no to pallets. Now... - Feb 12, 2020 by Evtimov
Hahaha we already praying.. There is always a solution for a... - Feb 12, 2020 by Djo
I see that the connector has plastic alignment pins. Is ther... - Feb 12, 2020 by SMTA-Alex SMTA
we are obliged by customer specifications that there will be... - Feb 13, 2020 by Djo
It may because the part weight is too high so a weight to co... - Feb 24, 2020 by sssamw
Traditionally these connectors are riveted to the board on h... - Feb 24, 2020 by sarason