Can we bent a PCB using mechanical force ?Will the PCB come ... - May 15, 2019 by dhanish
If you are trying to remove/reduce warpage in the PCB (I am ... - May 15, 2019 by charliem
Look up the glass transition temperature (Tg) for the PCB ma... - May 15, 2019 by Stephen
This issue is seen at mechanical process.The pcb is thin 32 ... - May 15, 2019 by dhanish
You really need to define what you mean when you say "b... - May 31, 2019 by Steve Thomas
Thanks Steve.The bent we are seeing is at the location witho... - Jun 01, 2019 by dhanish
It would kill the component on the opposite side, be careful... - Sep 23, 2019 by sssamw