Hi, we are experiencing insufficient solder and bridging so... - Nov 10, 2017 by myke_SMT
Just a few thoughts, as we use similar quite frequently with... - Nov 13, 2017 by PhilC
IMO – Look into nano-coatings for your stencil and radius ... - Nov 15, 2017 by Russfrom NH
Hello. We have a problem with QFN type. Component is elevate... - Dec 01, 2017 by Marks
It seems that it will work with 5 mil stencil. To be safe us... - Dec 01, 2017 by Evtimov
Stencil thickness is 4 mil. Via's are plugging from bottom. ... - Dec 01, 2017 by Marks
Brikainis, it looks like these vias are not plated and cl... - Dec 01, 2017 by Evtimov
EMIL, The first stencil was with 4 squares. then there wa... - Dec 01, 2017 by Marks
Very interesting pictures. It shows paste height of 200um - ... - Dec 01, 2017 by Evtimov
How about step down in the middle of thermo pad? I mean 0.0... - Dec 01, 2017 by Marks
Rework said that with hot air gun, heated the solder paste c... - Dec 01, 2017 by Marks
I am not sure that is doable. Ground Aperture is very small(... - Dec 01, 2017 by Evtimov
Recommended land and solder pattern says: VIA wall plating,... - Dec 01, 2017 by Marks
Have you ever heard of "Solder Mask Defined Thermal Pads"? ... - Dec 02, 2017 by Tom Hausherr
A new stencil has been purchased. to be continued. ... - Dec 04, 2017 by Marks