Hi, is there a reason why washing "no-clean" flux residue ... - Jul 20, 2016 by adamjs
Water washable no-clean flux works fine. Acetone, eew!!! ... - Jul 21, 2016 by davef
Acetone is flammable and hazardous to deal with. The fewer f... - Jul 21, 2016 by Tom
> Water washable no-clean flux Hrm, I have not heard of ... - Jul 21, 2016 by adamjs
> flammable and hazardous to deal with Just want to point... - Jul 21, 2016 by adamjs
Cleanable no-clean solder paste suppliers: * Yes, Kester ... - Jul 22, 2016 by davef
Acetone has hazards other than flammability and odor includi... - Jul 22, 2016 by Tom
I just wanted to point out that although acetone is GRAS the... - Jul 22, 2016 by Tom
> No recommendations ... Too many friends in the trade Fa... - Jul 23, 2016 by adamjs
> Acetone has hazards other than flammability and odor inclu... - Jul 23, 2016 by adamjs
I don't understand why you think I'm fear mongering simply b... - Jul 23, 2016 by Tom
Adam ... I like washable no-clean because it provides for pr... - Jul 27, 2016 by davef