Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3946
What could be the possible solution for shorted BGA but only... - Dec 22, 2014 by slouis2014
the most common reason can be popcorning of the device or wa... - Dec 23, 2014 by Bob Willis
The peak temp. during reflow is 285 degree, at this temperat... - Dec 23, 2014 by slouis2014
Assuming its 285 Celsius as measured at the solder joint, yo... - Dec 24, 2014 by JimPat
285 is way too high a temperature for a measured part or bal... - Dec 24, 2014 by Bob Willis
thanks for all the information. i will check on it. ... - Dec 28, 2014 by slouis2014