So I have this issue with my 1240. During my weekly oven s... - Mar 11, 2013 by Sr. Tech
I would check/replace the neighbour zones. If your temp isd ... - Mar 11, 2013 by Evtimov
Maybe I misinterpreted, because different people have differ... - Mar 11, 2013 by A Very Frazzled Man
The surveyor is a a plate that I use to "survey" or verify t... - Mar 11, 2013 by Sr. Tech
Not knowing XPM ovens , have zones are usually top heat and ... - Mar 13, 2013 by josh
I don't know your oven but I have dealt with high temperatur... - Mar 14, 2013 by sarason
The entire oven is clean there are no blockages and the heat... - Mar 14, 2013 by Sr. Tech