Hello folks, we would in certain cases run a PCB second t... - Jan 31, 2013 by Evtimov
Are you talking about double sided reflow or just multiple p... - Jan 31, 2013 by dontfeedphils
Let's say I have an open joint on a BGA and I want just to r... - Jan 31, 2013 by Evtimov
If you have a hard-gold on your pads, it's not a problem. Ha... - Feb 01, 2013 by ENIAC
Regardless of the surface finish, you should try to limit th... - Feb 01, 2013 by dyoungquist
Thank you guys. You keep adding valuable information here. I... - Feb 01, 2013 by Evtimov
In agreement with Evtimov. Max 5 reflow cycles. Something l... - Feb 01, 2013 by Hegemon
From some previous article I read (sorry, don't have citatio... - Feb 01, 2013 by isd.jww
Thank you all for the input. There is another concern. Do yo... - Feb 07, 2013 by Evtimov
I would consider wave solder as a cycle, in that for the mos... - Feb 07, 2013 by Hegemon
Hegemon, my thinking was pretty much the same. I will pro... - Feb 08, 2013 by Evtimov