We are having difficulty with bridging on a 2x50 pin 0.050" ... - Dec 06, 2012 by DeanM
no expert but would using a smaller diameter nozzle help in ... - Dec 07, 2012 by aj
I am no expert but would using a smaller nozzle help in anyw... - Dec 07, 2012 by aj
We had a similar issue and it was fixed by trimming the conn... - Dec 07, 2012 by Ken
We are using our selective solder machine to solder a backpl... - Dec 10, 2012 by dyoungquist
The issue is surface tension around the connector. Your tip... - Dec 11, 2012 by sarason
Thanks for the comments so far. The smallest nozzle I've tri... - Dec 11, 2012 by DeanM
Glad to hear we have more Jade users on the forum! What ... - Dec 12, 2012 by tombstonesmt
Nitrogen at nozzle supply is at around 47.5cfh. ... - Dec 12, 2012 by tombstonesmt
I had a connector like this and here is my recommendation: ... - Dec 19, 2012 by Evtimov
Hi, guys. Does anyone use a EBSO selective soldering mach... - Feb 26, 2013 by ENIAC