Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3104
I have read through the IPC/JEDEC J-STED-033.1 standards reg... - Oct 25, 2012 by mccabekev
4.2.7.1 states, ...If the bake temperature is not greater th... - Nov 06, 2012 by DeanM
Make sure that the 40 degree C oven is getting to less then ... - Nov 08, 2012 by Graham
For you info there is a maker of humidity cabninets in UK ca... - Nov 22, 2012 by josh