SACX0107 Solder for Wave

Views: 3408

#62060

SACX0107 Solder for Wave | 14 June, 2010

does anyone have experience with SACX0107 solder from Alphametals in Wave compared to SN100 or SAC305? I see better price and good features like less dross. However, the alloy looks like non-eutectic and it has 10 degree difference between liquidus and Solidus point. If you have experience with alloy, I'd appreciate your feedback. Thanks, sk

reply »

#62087

SACX0107 Solder for Wave | 19 June, 2010

hi I am Customer Support engineer for Alpha Metals.Attached is the doc , plz go through that.

Attachments:

reply »

ICT Total SMT line Provider

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes