We are a small Contract Manufacturer and have received a p... - Feb 25, 2010 by Duane
Good Afternoon Duane, Surface tension should be adequate ... - Feb 25, 2010 by CL
We agree with CL in the above posting. We talked about this ... - Feb 25, 2010 by davef
Good morning Chris, We had discussed surface tension but we... - Mar 01, 2010 by Duane
I don't think I would reduce the heat at all if there is n... - Mar 01, 2010 by WRONGWAY
So Far, so Good. Solder looks real good. Thanks ... - Mar 02, 2010 by Duane
Hi, Duane, Why don't you try Tacky Flux /Tacky paste flux... - Mar 04, 2010 by TACKY_TSF
How is that going to help hold a BGA to the bottom of the bo... - Mar 05, 2010 by kpm