Hello, since some days we are facing strange problem with S... - Aug 31, 2009 by d0min0
How do you go about and what happens when you rework the poo... - Aug 31, 2009 by davef
Have you profiled at the problem side of the part? ... - Sep 01, 2009 by isd.jww
davef As for the repair : - with hot air blower it is no... - Sep 01, 2009 by d0min0
Is the solder wetting to the pad, and not to the part? If s... - Sep 01, 2009 by robgd3
Because it's always the same terminal of the same part that ... - Sep 03, 2009 by isd.jww
Does the established joint still exist if once again re-touc... - Sep 03, 2009 by sachu_70
to summarize - 3 components are placed on a single module ... - Sep 03, 2009 by d0min0
Before you rule out the profile, did you run an actual profi... - Sep 19, 2009 by profilingguru
Did you try pre-tinning your board on this suspect pad/s to ... - Sep 22, 2009 by cman
hello, we are profiling with the pcb each day - results a... - Sep 23, 2009 by d0min0
Is it possible you are putting boards in the oven with littl... - Sep 23, 2009 by jdengler
that crossed our minds - overloading of the oven but in re... - Sep 24, 2009 by d0min0
I had this issue a few years ago with Kingbright LED's. The ... - Sep 24, 2009 by Mark