Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6460
We are using a water soluble flux which requires the assembl... - Jun 09, 2009 by dyoungquist
You're correct that JEDEC J-STD-033 defines baking condidtio... - Jun 10, 2009 by davef
Our cleaning process involves the assemblies being completel... - Jun 11, 2009 by dyoungquist
NASA recommends baking a PCB for a minimum of 4 hours at 93+... - Jun 11, 2009 by davef
Try immersing the assembly in IPA for 30 minutes. IPA is hy... - Jun 24, 2009 by Mark
Shanelo Technologies Given that isopropyl alcohol [IPA] i... - Jun 25, 2009 by davef
IPA is hydroscopic. ... - Jun 26, 2009 by Mark
He wants to "see underwater" ... - Jun 30, 2009 by charliem
But the boards and parts on the boards are also hygroscopic(... - Jul 01, 2009 by kpm