Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3421
Dear Sir. Recently we had a problem in our production. We h... - Jan 30, 2009 by Jose Luis
Buenas dias Jos�, It shoul not be a problem. We had situ... - Jan 30, 2009 by GSx
The concern about lead contamination of lead-free solder has... - Feb 01, 2009 by davef
Hi Jose, such a process is possible, but you need to confirm... - Feb 03, 2009 by sachu_70
Hi What is the surface finish you have? Following are true ... - Feb 03, 2009 by Milroy