Hi We have recently specified the following on a bareboa... - Oct 28, 2008 by Adam
Your gold might be a bit thin after you consider fabricator'... - Oct 28, 2008 by davef
Thanks for the feedback dave. What kind of problems am I lie... - Oct 29, 2008 by Adam
During soldering, the gold dissolves into the solder connect... - Oct 29, 2008 by davef
In addition to what Dave has said, you shouldn't worry much ... - Nov 01, 2008 by Vlad
Vlad, That was a bad statement to make... Enig should ... - Nov 03, 2008 by BoardHouse
We agree with Boardhouse that immersion gold inherently self... - Nov 03, 2008 by davef