I have a small board with some chips and 2 connectors (1 lar... - Apr 18, 2008 by sueph
Do you have a picture? SMTNet HAS the technology now to pos... - Apr 18, 2008 by Dirk Nuendyke
That you have 'grainy' solder only at the ends of the connec... - Apr 21, 2008 by davef
"Disturbed" usually means some form of movement. I would th... - Apr 21, 2008 by Real Chunks
Profiling can't happen outside of North Avenue. ... - Apr 21, 2008 by Peter Gibbons