Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 10117
Hi. I know that this is one of the mos common threads her... - Apr 09, 2008 by Manuel_R
what is your conveyor speed? stencil thickness? ... - Apr 09, 2008 by kircchoffs
conveyor speed: 30 in/min. 8 zones stencil thickness 6 mil ... - Apr 09, 2008 by Manuel_R
Is the stencil opening rectangular? Home Plate? What is the... - Apr 09, 2008 by elias
openings, rectangular no home plate. pad spacing don't have ... - Apr 09, 2008 by Manuel_R
We wonder about: * Solder mask encroaching onto the compone... - Apr 09, 2008 by davef
Stencil design and pad layout are key. Too far apart - bad.... - Apr 10, 2008 by Dirk Nuendyke
If I read you right the issue is mostly with components from... - Apr 10, 2008 by ScottE
Umm.... he states he is using the Induium paste for 2 weeks ... - Apr 10, 2008 by Real Chunks
Update: Recently, we ran a (old) product on which they ma... - Apr 14, 2008 by Manuel_R
Many factors will make tombstone happen. from design/stencil... - Apr 22, 2008 by fowlerchang
Here is my email as below: ... - Apr 22, 2008 by fowlerchang
It is CSP reliability issue, which is the mobile CPU from Sp... - Apr 22, 2008 by fowlerchang