Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 8157
Hi all! Heres wishing everyone a Happy & Prosperous 2008!! ... - Jan 03, 2008 by fsw
Q1: Can Stainless steel be soldered? A1: Yes, stainless ste... - Jan 03, 2008 by davef
Davef, thnx for your reply. Sorry, forgot to clarify "our no... - Jan 03, 2008 by fsw
Patrick, thnx for your info. The tabs will be soldered on a ... - Jan 03, 2008 by fsw
Stainless steel can NOT be soldered with the solder that is ... - Jan 03, 2008 by Dirk Nuendyke
Recommended procedure for soldering stainless steel [Atlas S... - Jan 03, 2008 by davef
Consider conductive epoxy. Among the suppliers that make the... - Jan 03, 2008 by davef
Why are you using stainless steel? Corrosion resistance? Ca... - Jan 03, 2008 by Flipit
So, I'd have to grind the living sh#t out of my wedding ring... - Jan 04, 2008 by Dirk Nuendyke
All, The reason SS (stainless steel) was being considered... - Jan 04, 2008 by fsw
Good move. Again, stainless can NOT be soldered with standa... - Jan 04, 2008 by Dirk Nuendyke
they make tin plated steel batt contacts. may be your best o... - Jan 07, 2008 by RDR
Another thing I'm curious about. What is the "functional pu... - Jan 07, 2008 by Dirk Nuendyke
All must be cautioned when messing with acids. Of course, ne... - Jan 07, 2008 by mparker
might try solder-less through hole connector technology for ... - Jan 07, 2008 by mparker
If your wedding ring ever gets hot enough to melt solder, I ... - Jan 08, 2008 by jmelson