Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 46581
Are there significant diffrences in terms of soldering (wire... - May 30, 2007 by GSx
At the end of the day, you won't notice a difference, while ... - May 31, 2007 by davef
Tnks Davef, be patient pls, what does it exactely mean... - May 31, 2007 by GSx
In addition to Dave�s response: RO fluxes are based on na... - May 31, 2007 by Patrick Bruneel
Tnks Patrick, additional infos..... we are just playng... - May 31, 2007 by GSx
Let me give you some good advice You take already plenty... - May 31, 2007 by Patrick Bruneel
LOL... you need a break dave! MACGBWL! ... - May 31, 2007 by WaveMasterLarry
Thank Patrick for your infos. Seen that youa are an expet... - May 31, 2007 by GSx
Thanks Patrick, also IPC-HDBK-001 explains even better th... - Jun 01, 2007 by GSx