I have a customer that designed a fine pitch BGA into a boar... - Mar 14, 2007 by
We had a customer do a similar thing. We notified our custo... - Mar 15, 2007 by
Ask the board fabricator to: * Fill the vias with resin. *... - Mar 16, 2007 by davef
Hello, those plated and solderable via in pads have two c... - Mar 23, 2007 by
Shane