Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6199
There are several smd components in our factory that don't r... - Jan 25, 2007 by
Are you running a lead free process? If not, have you identi... - Jan 25, 2007 by Steve Thomas
We are using tin-lead solder. The components could be lead ... - Jan 25, 2007 by
Good luck with that. ;) More likely you'll have to adjust... - Jan 25, 2007 by Steve Thomas
Wagoner, Try switching to a transitional paste designed f... - Jan 25, 2007 by Real Chunks
You should have no problem using lead-free components with t... - Jan 26, 2007 by dyoungquist
We reflow with hot air. Our peak reflow temp is 220 to 225 ... - Jan 29, 2007 by
Print your paste onto a ceramic tile, place the offending co... - Jan 30, 2007 by
We've had multiple issues with non-wetting components. You ... - Jan 31, 2007 by
wagoner