Hi, I am having problems reworking a lead free PBGA (23mm... - Jan 17, 2007 by
When placing the part to be reflow try applying heat to the ... - Jan 17, 2007 by Jaime39
appears to be incomplete reflow on a couple of balls or they... - Jan 17, 2007 by RDR
So you are suggesting to begin heating using a preheater onl... - Jan 18, 2007 by
Thanks. I will turn off the machine activated cooling and h... - Jan 18, 2007 by
won;t recommend a paste since I propose that you do not use ... - Jan 18, 2007 by RDR
Thanks Russ. I meant paste flux or as some refer to it tack... - Jan 18, 2007 by
yeah Jeff, i would make sure that you are not overheating pa... - Jan 19, 2007 by RDR