Hello Experts, is it acceptable in IPC standard to have t... - Mar 19, 2019 by PCB
why wouldn't you just drill one larger hole? ... - Apr 19, 2019 by cbart
It's a terrible idea. Through holes should be drilled in the... - Apr 19, 2019 by davef