We are deciding on using SN100C on leadfree wave soldering p... - Mar 24, 2006 by Mike H
Mike, I have to inform you that if you don�t let "sales p... - Mar 28, 2006 by Patrick Bruneel
SN100C, not as aggressive towards other metals as are other ... - Mar 28, 2006 by Steve
Who exactly is "we". ... - Mar 28, 2006 by RDR
That's what I was trying to find out ... - Mar 28, 2006 by RDR
Oh no you caught me. I'm a salesperson. "We" refers to the d... - Mar 28, 2006 by Steve
Its all good steve! We had you pegged. It shows something ... - Mar 28, 2006 by RDR