effect of copper

Views: 2276

#78064

Effect of copper | 4 July, 2017

Hi Everyone

I wonder know the effect of copper in solder paste, solder bar.

Thanks.

reply »

#78085

Effect of copper | 5 July, 2017

You've posed a very broad question, I'm not sure what you're asking.

As a starting point ... Kester reported “The Effect Of Metallic Impurities On The Wetting Properties Of Solder“ [http://www.smtnet.com/library/index.cfm?fuseaction=view_article&article_id=820&company_id=41186]

reply »