Electronics Forum | Fri Sep 06 03:11:31 EDT 2013 | 5pcb
Welcome phone call from all over the world.
Electronics Forum | Fri Sep 06 03:06:18 EDT 2013 | 5pcb
We are a complex pcb supplier in China. We are good at making prototypes and multilayer (8-20)layers PCB. If you think your boards are difficult enough, you can contact me. Let's talk details. sales2@dmele.com Name:Lily Tel:0086-0755-23006293.
Electronics Forum | Wed Jun 20 16:03:01 EDT 2001 | Gil Zweig
The multi-layer printed circuit board manufacturers have been using x-ray inspection for many years to quality control drilling and lamination of multi-layers. Assemblers should consider using x-ray for incoming quality control from their multi-layer
Electronics Forum | Mon Dec 18 18:08:41 EST 2000 | Dave F
What are the issues with fabricating multilayer PTFE boards? Are these compare with the issues of throught holes and vias in PTFE boards? If not what are these issues?
Electronics Forum | Wed Feb 25 07:55:27 EST 2015 | 3dpcb
We're developing a 3D printer for professional multi-layer PCBs with 3-4 Mil. traces. What concerns or questions would you have about such a system?
Electronics Forum | Tue May 27 12:53:15 EDT 2003 | davef
Our solder irons are tuned to 700*F, but the in-use temperature varies according to the solder alloy and the characteristics of the board and components. Check some of the papers on multilayer ceramic capacitors. They get fairly specific, for insta
Electronics Forum | Tue Jan 15 10:19:39 EST 2013 | boriskilk
For a multilayer board the thickest internal copper layer we will do is 0.062".
Electronics Forum | Thu Aug 10 13:36:48 EDT 2000 | Bob Willis
I recently have been examining multilayer board failures. They are the classic inner connection failure between the foil and the through hole plating which I have not seen in many years. Has any one experienced any issues recently specifically relati
Electronics Forum | Thu Aug 11 16:24:16 EDT 2005 | Sue PH
The soldering handbook that I use gives a 'rule of thumb' for best preheat temps for wave soldering. For multilayer brds that are metal core it suggests 110 to 130 degrees C topside temp to get the best solder fillet. We do a lot of multilayer meta
Electronics Forum | Fri Nov 17 14:36:17 EST 2006 | Fer
Good afternoon all, There is an issue in my company regarding flatness on SMDs. The part I am fabricating is a multilayer assembly of .175" by .175" by .049" thick. The part is made out of a multilayer copper clad PTFE with a tin finish surface. Af