Stencil apertures IPC design | 24 February, 2006

What is the IPC norm wich drives the IPC stencil aperture design? The contest is: a stencil for the deposition of solder pastes on bare boards

Thanks

reply »

#40046

Stencil apertures IPC design | 28 February, 2006

The key driver to aperture design is to assure a fillet of the proper height for the component temination and the reliability of the end-product customer use environment.