what is the required storage temp. for litz wire

Views: 1263

arnold

#38916

what is the required storage temp. for litz wire | 9 January, 2006

Cmiller

#39018

what is the required storage temp. for litz wire | 12 January, 2006

The mfg. should be able to tell you. We store ours, for winding transformers, at room temperature. Have had no issues.