Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


MPP4202 diodes from Microsemi

Views: 1107

John

#38387

MPP4202 diodes from Microsemi | 12 December, 2005

I'm having problems feeding these to the pick and place. As the tape peels off the pocket the part sticks to the tape rather than remaining in the pocket.

Machine is QUAD QSV. We've tried all generations of feeders we have available.

Any advice is appreciated.

reply »

bobpan

#38389

MPP4202 diodes from Microsemi | 12 December, 2005

Sounds like too much adhesive on the tape or static electricity. Try grounding the feeder if you think its not adhesive/tape related.

reply »