Antistatic | 24 November, 2005

We are using QFP & other IC's in SMT but not using the antistatic pecautions.

I want to know that what effect can be on IC's in future. Because we did not get any IC damege immidiatly. How long after this will affact the IC,s.

reply »

#38073

Antistatic | 24 November, 2005

It's a good question. These are the expensive failures you want to avoid, because your customer finds them. [It's easy to find the cheap failures, those that you find before they leave your plant.] Google "esd latent damage" to begin your investigation.