cap size and copper thickness vs part size questions | 7 November, 2005

If I am putting chip capacitors on a .063 FR4 board, what size package should we stay away from to avoid cracking?

If I use 2 mil copper on the outside layers of a PCB, am I limited to what pitch of parts I can use? Specifically, will using 0603 caps or parts with .65mm pin spacing cause problems?

reply »

#37850

cap size and copper thickness vs part size questions | 14 November, 2005

Ceramic capacitors larger then EIA size 1812 are known to be very susceptible to thermal shock damage due to their large ceramic mass.