wave solder bath coating - leadfree purposes.

Views: 865

Adnahn

#37685

wave solder bath coating - leadfree purposes. | 7 November, 2005

Please advise if Plasma Nitride for Stainless Steel is suitable or a proposed method to coat the wave solder bath for leadfree.

Thanking you in advance.

Regards, Adnahn

reply »

slthomas

#38174

wave solder bath coating - leadfree purposes. | 1 December, 2005

I'm going to attempt to resurrect this thread because a recent development has me interested too. Anyone experienced in this with respect to durability, cost, etc.?

reply »