Electrical shorts on glass frit seal of ceramic ICs

Linda Woody

#34011

Electrical shorts on glass frit seal of ceramic ICs | 2 May, 2005

Has anyone experienced electrical shorting between adjacent leads of a ceramic hermatic sealed IC? If so, can you share root cause and corrective action? The shorting appears to be in the glass frit seal itself but the failure mechanism is unknown. Any similar experiences that can be shared would be greatly appreciated.

Thanks - Linda

reply »

KEN

#34054

Electrical shorts on glass frit seal of ceramic ICs | 3 May, 2005

Tin wiskers

Electro migration

all in the same week! (just kill me now God)

reply »

jimby

#34114

Electrical shorts on glass frit seal of ceramic ICs | 6 May, 2005

Make sure that whoever is pretinning leads are not using a water soluble flux. If they are, make sure parts are being cleaned immediately upon cooling