Device Falloff

Haran

#33505

Device Falloff | 3 April, 2005

We have received a board from our customer with one of the Transformer falling off.The component lead plating fell off but there is solder fillet at the PCB pad is good.

reply »

zsolt

#33514

Device Falloff | 4 April, 2005

That's bad. But WHAT IS THE QUESTION ? :)

reply »

Haran

#33524

Device Falloff | 4 April, 2005

What could be the cause?The lead plating is Nickel and Tin.

reply »


RDR

#33526

Device Falloff | 4 April, 2005

I would bet that you never wetted to the nickel.

reply »