we are having problem with the flipchip sticking to the tape and reel cover, jumping around the tape pockets, and double stacking at placement during production. Does anybody else have this problem? Does anybody have a solution.

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#32753

Flipchip sticking to tape and reel covers | 19 February, 2005

Potential causes are: * Static charge [get a deionizing fan] * Adhesive on the inside of the cover tape [fix your supplier]

reply »

#32760

Flipchip sticking to tape and reel covers | 21 February, 2005

Agree with Davef. Smaller the chip, more the static charge. I used to see this even with normal chips. Get an ionizer blow. It should solve your problem. May be switch to antistatic tape if affordable.Regards. GV

reply »

need help

#32783

Flipchip sticking to tape and reel covers | 21 February, 2005

Thanks for your help. We try the de-ionizer fan, helps some what but did not eliminate the problem. Can you tell me which model are you guys using.