soldering lead free component with lead bearing solder

steve

#32600

soldering lead free component with lead bearing solder | 11 February, 2005

I know this has been dealt with in the past but I couldn't dig up anything in the archives. If I'm soldering a 0402 lead free component with 63/37 solder is this a problem. Also lets take the opposite. If I'm soldering a lead bearing 0402 with lead free solder is this a problem. One of these scenarios is not good but I forgot which one and WHY? thanks for any assistance.

reply »

#32612

soldering lead free component with lead bearing solder | 12 February, 2005

Here's one thread from the fine SMTnet Archives: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=30307