DEK 265GS

Randy Gray

#32497

DEK 265GS | 8 February, 2005

Does any one know the fine pitch print capability on a DEK 265GS?? Thank you

reply »

aj

#32511

DEK 265GS | 9 February, 2005

Randy,

We have a Dek 265GSX and 265 MK1. We print 20thou pitch components, 0.5mm.

Just make sure you have good board support and USC.

aj

reply »

#32512

DEK 265GS | 9 February, 2005

With a properly designed and maintaned stencil, good solderpaste and board supports on the printer you can even go down to 0.4mm (16mil) with good results.

reply »