Looking for 93.5 PB 3 SN 1.5 AG

Joel Dudley

#31627

Looking for 93.5 PB 3 SN 1.5 AG | 9 December, 2004

I'm hoping to find someone out there who has some no clean, 93.5 PB, 3 SN, 1.5 AG, .015 Diameter. If you have some and are willing to part with it please let me know.

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »


RDR

#31629

Looking for 93.5 PB 3 SN 1.5 AG | 9 December, 2004

Indium has some alloys that are very close to this but not exactly. You may want to contact them if nothing shakes loose from here.

www.indium.com

Russ

reply »

#31630

Looking for 93.5 PB 3 SN 1.5 AG | 9 December, 2004

This is a perculiar alloy. Usually, the portions of each metal in the alloy sum to 100. Yours sums to 98. Could you be seeking 93.5Pb 5Sn 1.5Ag? It is more available.

reply »

Joel Dudley

#31633

Looking for 93.5 PB 3 SN 1.5 AG | 9 December, 2004

Sorry about that. It is supposed to be a 5 SN. I typo'd.

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#31642

Looking for 93.5 PB 3 SN 1.5 AG | 9 December, 2004

Try: http://www.cranesolder.com

Also, maybe ESL, in addition to Indium that Russ mentioned.

reply »