Ceramic Inks



Ceramic Inks | 23 September, 2004

Can ceramic inks be used as conductive ink as a substitue of silver inks

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »


Ceramic Inks | 28 September, 2004

We use "0" ohm resistors a links. Is that what you're talking about?

reply »



Ceramic Inks | 30 September, 2004

i am talking about ceramic conductive inks(which contain silver particles)