#29594

siemens nozzles cracking | 22 July, 2004

Can some one explain to me why the ceramic nozzles are cracking not on the tip but on the base??? also how long do the sleeves last, no informaton from siemens they just came in and changed from 'o'ring to bearing type??

Thanks Julie

reply »

#29595

siemens nozzles cracking | 22 July, 2004

Hi julie I found that it was the sleeve on the ball bearing that was the fault we went back to the oring type problem gone.

reply »

Jeff

#29665

siemens nozzles cracking | 26 July, 2004

Sounds to me like a nozzle changer issue; broken garages or needs to be calibrated?